PPS/R-5
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
基本性能 | 吸水率 | ASTM D-570 | 0.05 | % | ||
物理性能 | 比重 | ASTM D-792 | 1.72 | |||
PPS/R-5机械性能 | 伸长率 | ASTM D-638 | 1.0 | % | ||
IZOD冲击强度 | 3.2mm厚有缺口 | ASTM D-256 | 9 | Kg.cm/cm | ||
3.2mm厚无缺口 | ASTM D-256 | 38 | Kg.cm/cm | |||
抗压强度 | ASTM D-695 | 1820 | Kg/cm2 | |||
抗折模数 | ASTM D-790 | 17×104 | Kg/cm2 | |||
洛氏硬度 | ASTM D-785 | 123 | R-SCALE | |||
抗折强度 | ASTM D-790 | 2260 | Kg/cm2 | |||
抗拉强度 | ASTM D-790 | 1620 | Kg/cm2 | |||
PPS/R-5电气性能 | 介电损耗正切 | 1KHz | ASTM D-150 | 0.002 | ||
体积固有电阻率 | ASTM D-257 | 1×1016 | Ω.cm | |||
绝缘破坏电压 | ASTM D-149 | 17.2 | KV/mm | |||
耐电弧性 | ASTM D-495 | 128 | Sec | |||
介电损耗正切 | 1MHz | ASTM D-150 | 0.0014 | |||
介电常数 | 1MHz | ASTM D-150 | 3.9 | |||
介电常数 | 1KHz | ASTM D-150 | 4.0 | |||
加工性能 | 成型收缩率 | ASTM D-955 | 0.002 | cm/cm | ||
PPS/R-5热性能 | 热变形温度 | 18.6kg | ASTM D-648 | 260 | ℃ | |
燃烧性 | UL 94 | V-0 | ||||
导热系数 | 0.25 | Kcal/m.Hr℃ | ||||
线热膨胀系数 | ASTM D-696 | 2.7 | ×10-5cm/cm/℃ | |||
UL温度指数 | UL | 200(220) | ℃ |