C | Si | Mn | P | S | Cr | Mo | W | Ni | V | Nb | N | |
0Cr13Ni4-6MoRe | ≤0.06 | ≤1.0 | ≤2.0 | ≤0.03 | ≤0.03 | 12-14 | ≤1.0 | / | 3.5-6.5 | / | / | / |
00Cr13Ni4-6MoRe | ≤0.03 | ≤1.0 | ≤2.0 | ≤0.03 | ≤0.03 | 12-14 | ≤1.0 | / | 3.5-6.5 | / | / | / |
ER414L | ≤0.03 | ≤1.0 | ≤2.0 | ≤0.03 | ≤0.03 | 12-14 | ≤1.0 | / | 4.5-5.5 | / | / | / |
ER415L | ≤0.03 | ≤1.0 | ≤2.0 | ≤0.03 | ≤0.03 | 12-14 | ≤1.0 | / | 4.5-5.5 | / | / | / |
ER416L | ≤0.03 | ≤1.0 | ≤2.0 | ≤0.03 | ≤0.03 | 15-17 | ≤1.0 | / | 4.5-5.5 | / | / | / |
ER414L(T) | ≤0.03 | ≤0.8 | ≤1.0 | ≤0.02 | ≤0.008 | 12-13.5 | 0.6-0.9 | / | 3.8-4.5 | / | / | / |
ERP91 | 0.07-0.14 | ≤0.50 | ≤1.20 | ≤0.01 | ≤0.01 | 8.0-10.5 | 0.7-1.20 | / | ≤1.0 | 0.15-0.30 | 0.02-0.10 | 0.02-0.07 |
ERP91W | 0.07-0.14 | ≤0.50 | ≤1.20 | ≤0.01 | ≤0.01 | 8.5-10.5 | 0.7-1.20 | 0.90-1.60 | 0.4-1.0 | 0.15-0.30 | 0.02-0.10 | 0.02-0.07 |
材料牌号 | 抗拉强度 | 屈服强度 | 延伸率 | 冲击韧性 | HV |
0Cr13Ni4-6MoRe | ≥760 | ≥550 | ≥15 | ≥50 | ≤285 |
00Cr13Ni4-6MoRe | |||||
ER414L、ER415L、ER416L | ≥760 | ≥550 | ≥15 | ≤300 |
材料牌号 | Akv2(J) | 热处理状态 | ||||
ERP91、ERP91W | ≥620 | ≥530 | ≥17 | ≥40 | 47/38平均值/低值 | 740±10℃×4h |
牌号 | 主要用途 | 主要性能 |
0Cr13Ni4-6MoRe | 主要用于同材质铸钢件的补焊和水电站过流部件汽蚀磨损后的堆焊修复以及同材质结构件的焊接。 | 为低氢型药皮马氏体不锈钢焊条。堆焊金属具有良好的抗汽蚀耐泥沙磨损性能。焊条焊接工艺性能良好,采用直流反接,适合于全位置焊接。堆焊工艺简单,焊前不预热,焊后不用热处理,堆焊层可以切削加工。 |
00Cr13Ni4-6MoRe | ||
ER414L(T)、ER414L、ER415L | 用于同材质铸钢件的补焊和水电站过流部件汽蚀磨损后的大面积堆焊修复以及水轮机过流部件的制造焊接。 | 为马氏体不锈钢气保护焊丝,纯氩保护或富氩气体保护,具有X良的焊接工艺性能。 |
ER416L | 为三相不锈钢气保护焊丝,纯氩保护或富氩气体保护,具有X良的焊接工艺性能。 | |
ERP91 | 适用于X(X)临界汽轮机高压汽缸ZG1Cr10MoVNbN及T/P91管道用耐热钢的焊接。 | 马氏体耐热钢实芯焊丝,焊丝工艺性能良好,具有X良的熔敷金属机械性能。 |
ERP91W | 适用于改进型GX12CrMoWVNbN耐热钢焊接。 | 马氏体耐热钢实芯焊丝,焊丝工艺性能良好,具有X良的熔敷金属机械性能。 |
牌号 | 类别 | 符合标准 | 规格 |
0Cr13Ni4MoRe 0Cr13Ni5MoRe 0Cr13Ni6MoRe | 焊条 | AWS E410NiMo | Φ3.2、φ4.0、φ5.0 |
00Cr13Ni4MoRe 00Cr13Ni4MoRe 00Cr13Ni4MoRe | AWS E410NiMoL | Φ3.2、φ4.0、φ5.0 | |
ER414L(T)、ER414L、ER415L | 气保护焊丝 | AWS ER410NiMo(L) | Φ1.2 |
ER416L | Φ1.2 | ||
ERP91 | AWSER90S-B9 | Φ1.2 | |
ERP91W | AWSE9015-B9 | Φ1.2 |